NS335 Corrosion Resistance Alloy Steel Pipe
NS335 is resistant to chloride ion oxidation-reduction composite corrosion alloy, the good thermal stability of the organization. Wet chlorine, hypochlorous acid, sulfuric acid, hydrochloric acid, mixed acid, chloride device, after welding directly applied.