GH536 High Temperature Alloy Steel bar

 

GH536 superalloy is a nickel-chromium-molybdenum alloy with cobalt and tungsten added. GH536 alloy in high temperatures up to 1200 ℃ has excellent oxidation resistance, can also be applied to the neutral and reducing atmosphere. At the same time, GH536 alloy can resist carbonation and nitriding atmosphere.

● Excellent oxidation resistance at temperatures up to 1200 ° C

● High-temperature strength

● good formability and weldability


● good resistance to stress corrosion cracking