Incoloy refers to a range of superalloys produced by the Special Metals Corporation group of companies. They are mostly nickel-based, and designed for excellent corrosion resistance as well as strength at high temperatures; there are specific alloys for resistance to particular chemical attacks (e.g. alloy 020 is designed to be resistant to sulphuric acid, DS to be used in heat-treating furnaces with reactive atmospheres and many heat cycles)

Incoloy MA956 is made by a mechanical alloying rather than a bulk-melting process; it was studied for space reactor components in the JIMO project. It is difficult to weld and needs to be heated to 200C for cold-forming processes.