54SiCr6 Spring Steel Bar


54SiCr6(DIN) is added Si-Cr to enhance after heat treatment performance spring steel. Used for strained springs for cars and railway carriages and for surfaces requiring abrasion resistance. High strength, hardness and wear abrasion resistance. Low machinability, workability and weldability.

 

Chemical Composition:

 

C(%)Si(%)Mn(%)P(%)S(%)Cr(%)Ni(%)Cu(%)
0.51-0.591.20-1.600.50-0.80≤0.03≤0.030.50-0.80--

 

Mechanical Properties:

 

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV/Ku (J)
Elongation
A (%)
Reduction of area ψ (%):hardness (HB)
≥13001450-2050Min.8≥ 6≥ 25Max. 280

 

Physical Properties:

 

Temperature
(°C)
Modulus of elasticity
(GPa)
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) andThermal conductivity
(W/m·°C)
Specific thermal capacity
(J/kg·°C)
Specific electrical resistivity
(Ω mm²/m)
Density
(kg/dm³)
Poisson’s coefficient, ν
22--  0.21- 
866524-24.3411 - 
485-1433.2  412313

 

54SiCr6 Technical Data Sheet PDF .